Inconel 625 vs Hastelloy C-276 for Chlorides

Both survive seawater. They fail differently in hot chloride-bearing process streams. A working sequence for UNS N06625 and UNS N10276.

Why this comparison keeps coming up

Inconel 625 (UNS N06625) and Hastelloy C-276 (UNS N10276) are the two grades most often offered for the same chloride-bearing duty. Both are nickel-base, both are normally supplied in the solution-annealed condition, both weld without preheat, and both appear on mill stock lists in bar, plate, tube and forging form. A distributor will often quote either one. They are not interchangeable, and the difference is not a matter of one being better. It is a matter of which failure mechanism the service will actually produce.

625 is a nickel-chromium-molybdenum-niobium alloy strengthened mainly by solid-solution hardening from molybdenum and niobium, with roughly 20 to 23% chromium, 8 to 10% molybdenum and 3.15 to 4.15% niobium plus tantalum under ASTM B 443 for plate, B 446 for rod and bar, and B 564 for forgings. C-276 is a nickel-chromium-molybdenum alloy with about 14.5 to 16.5% chromium and 15 to 17% molybdenum, with deliberately low carbon and silicon, specified to B 575 for plate, B 574 for bar and B 564 for forgings, and B 622 for seamless tube. The single most useful number in this comparison is the molybdenum: roughly twice as much in C-276.

The mechanism, not the grade name

Chloride attack is localised. It opens pits at the passive film and then concentrates inside crevices, under gaskets, beneath deposits and in the heat-affected zone of a weld. General corrosion rate tables are almost useless for predicting it. The relevant comparison is resistance to pitting and crevice initiation at the actual service temperature, in the actual oxidising or reducing condition, with the actual contaminants present.

In ambient seawater and in many oxidising chloride environments, 625 performs very well and has a long record in marine and offshore hardware; its higher chromium supports a robust passive film. C-276 was designed for reducing and mixed acid-chloride conditions where that passive film is not stable — hydrochloric acid, wet chlorine, mixed acid streams and reducing media contaminated with chloride. Its high molybdenum and tungsten content is what carries resistance when chromium passivity cannot be relied on. In those conditions 625 can pit and crevice-corrode while C-276 survives.

Temperature decides which of those two situations you are in. A stream that is harmless at 30 °C can become aggressive at 90 °C, and crevice corrosion has a threshold temperature that is specific to the alloy and to the crevice geometry. Two figures are worth asking a supplier for: the critical pitting temperature and the critical crevice temperature measured in a defined test solution, and the ASTM G 48 method used to obtain them. A grade quote without those numbers is a chemistry quote, not a corrosion qualification.

Mechanical and fabrication differences that change the decision

625 in the annealed condition has a minimum yield strength in the range of roughly 275 to 415 MPa depending on product form, condition and section, and it retains useful strength at elevated temperature; it is also widely used as a weld overlay and cladding filler because it deposits cleanly. C-276 in the annealed condition is typically around 283 MPa minimum yield and is normally chosen for corrosion resistance rather than for load. If the part is a pressure boundary that must carry load as well as resist corrosion, 625 or a precipitation-hardened grade may be the better starting point, and where strength at temperature dominates, 718 enters the comparison.

Both grades weld by GTAW and GMAW with matching filler, low heat input and no preheat, but they punish poor practice differently. 625 is sensitive to hot cracking when a weld is heavily restrained and niobium-bearing constituents segregate in the interdendritic regions. C-276 is sensitive to precipitation of intermetallic phases if it is held in the 600 to 1000 °C range, which is why heat input and any post-weld thermal exposure are controlled. For either grade, specify the filler by AWS classification and require the corrosion test on the welded coupon, not only on the base metal.

A working selection sequence

A note on PREN: the formula %Cr + 3.3(%Mo) + 16(%N) is written for stainless and duplex grades. Applying it as a ranking shortcut to two nickel-base alloys is tempting and misleading; solid-solution nickel alloys do not owe their resistance to the same passive-film mechanism, and a single index cannot substitute for a corrosion test in the real medium. We mention it because it appears on many supplier datasheets, not because we use it to choose between 625 and C-276.

Send us the medium, the temperature range, the contaminants, the crevice geometry and the drawing. We will propose the grade and the governing specification together — and we will say plainly when neither grade is the right answer and a lined vessel or a different alloy family is.

Machined nickel alloy ring and flange components on the ROBAN floor
Finished components machined from certified bar and forging stock.

Related grades and specifications: Inconel 625 · Hastelloy C-276 · ASTM B 564

More

More from this section